Prime Tuff-X 200 HG offers the same great benefit as our Tuff-X 200 but also has a very high gloss before and after forming. Using the Gardner Gloss Meter at 60º angle gloss levels of 85 to 90 have been obtained after forming. Applications: This combination of materials is ideal for such applications as automotive, power tools, irrigation, fluid handling, lawn and garden, electronics, RV Interior and exterior parts. Information provided by Primex Plastics Corporation |