MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Reynolds EpoxAcast® 655; Hardener: HT High Temp Aluminum filled castable epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Cast, Metal Filled

Material Notes: Product Overview: EpoxAcast™ 655 (formerly Metalset™ A-30) is a versatile aluminum filled castable epoxy that is very hard and strong. It is dimensionally stable, even when mass cast up to 512 in3/ 8,390 cm3. Different hardener speed options are available depending on your project requirements. Maximum heat resistance is achieved using HT HIGH TEMP hardener (up to 225°F/108°C). Cured EpoxAcast™ 655 epoxy has high physical properties and is used for a variety of applications including making hard tooling, vacuum forming dies/molds, injection molds, foundry patterns, jigs and fixtures and metal forming dies. Depending on project requirements, Part A Base can be mixed with 101 FAST, 102 MEDIUM, 103 SLOW or HT HIGH TEMP hardeners.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.64 g/ccASTM D-1475
Viscosity 12000 cPMixed; ASTM D-2393
Linear Mold Shrinkage 0.0010 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90ASTM D-2240
Tensile Strength, Ultimate 6000 psiASTM D-638
Elongation at Break 0.50 %ASTM D-638
Tensile Modulus 7.20e+6 psiASTM D-638
Compressive Strength 15700 psiASTM D-695
Compressive Modulus 270000 psiASTM D-695
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 108 °CDeflection Temp. Post cured per heat post curing schedule; ASTM D-648
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour24 Hours followed by: Heat cure for 2 hrs. at 175°F/80°C, then 3 hrs. at 300°F/150°C.
Pot Life 240 minASTM D-2471
 
Descriptive Properties
ColorGrey
Mix Ratio100A:8Bby weight
Specific Volume16.5[in3/lb], ASTM D-792

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN199 / 296900

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.