MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Lanxess Vulkanol® OT Rubber Plasticizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Vulkanol® synthetic plasticizers are required as active ingredients to adjust the properties of vulcanizates, for example, to reduce hardness, modulus and tensile strength or to increase ultimate elongation and resilience. Certain grades contribute to special properties such as improved low temperature flexibility or enhanced green tack of compounds. As a processing aid, plasticizers reduce compound viscosity and improve flow during processing, which results in lower processing temperatures and power consumption.

Key Properties:

  • Improves processing behavior
  • influences important vulcanizate properties
  • contributes to special properties such as low temperature flexibility

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 - 0.980 g/ccDIN 51 757
Viscosity 19 - 29 cPDIN 53019
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.471 - 1.477DIN 51423
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
Appearancenearly colorless to yellow liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY9155 / 209546

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.