MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lanxess Uniplex FRP 44-94 Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Uniplex FRX 44-94 is a powdery flame retardant. The nitrogen and phosphorus blend components form an intumescent layer under heat and fire exposure. It is used as an intumescent flame retardant in thermosets, polyolefin compounds as well as in paints and coatings. Uniplex FRX 44-94 offers an excellent UV stability. In addition the product is non-hydroscopic. It can be processed at temperatures up to 225°C.

Chemical name: Nitrogen and phosphorus containing blend

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption <= 0.15 %<= 0.15 %
Particle Size <= 14 µm<= 14 µm90%
 
Thermal PropertiesMetricEnglishComments
Melting Point 254 °C489 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 36.0 Month36.0 Month
 
Component Elements PropertiesMetricEnglishComments
Nitrogen, N 27 %27 %
Phosphorus, P 15.7 %15.7 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 30 wt.% glass
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 20 wt.% glass
Lanxess Uniplex FRP-45I Plastic Additive
Lanxess Uniplex FRP-45 Plastic Additive
C-Glass Fiber, Generic

PLANY9122 / 209513

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.