MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Durez®-ter S1172-210 Polyester Polyol
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Durez® -ter S1172 is a hydroxyl terminated polyester diol series, designed for application in polyurethanes. Durez® -ter S1172- 110 is a fully saturated material based on dibasic acid and a glycol.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.020 %EST 4
 
Chemical PropertiesOriginal ValueComments
Acid Value 0.50[mg KOH/g]; EST 6
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 20APHA; EST 2
 
Descriptive Properties
Hydroxyl Number210[mg KOH/g]; test method: EST 3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Haysite HTF Polyester, High Temp Flex
Saint-Gobain Quartzel® Fabric/Cyanate Ester Resin Composite
Saint-Gobain Chemlam® RL® RL1000 PTFE-Coated Polyester/Cotton Blend Reinforced Laminate
Sumitomo Bakelite Durez®-ter S1011-210 Polyester Polyol
Sumitomo Bakelite Durez® 25378 Phenolic, Injection Grade

PSUMIT411 / 194216

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.