MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Oppalyte™ 40MD447 OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: A coextruded super white opaque, modified higher density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for use on VFFS and HFFS machines.

Availability: Africa & Middle East, Asia Pacific and Europe

Key Features:

  • Exceptional stiffness and flex resistance
  • Good seal strength
  • Excellent dimensional stability
  • Good hot slip
  • Good hot tack
Features:
  • In Lamination Lap Sealable
  • Light Barrier
Applications:
  • Bakery
  • Biscuits/Cookie/Crackers
  • Confectionery, Chocolate
  • Confectionery, Gum
  • Confectionery, Sugar
  • Crisps and Snacks
  • Dry Foods and Beverage Powders
  • Fresh Produce
  • Frozen Food
  • Health and Beauty Care
  • Household and Detergents
  • Ice Cream
  • Pet Food
Uses:
  • Box Overwrap Flexible Packaging
  • HFFS Flexible Packaging
  • Pre-made Bags – Flexible Packaging
  • VFFS Flexible Packaging
Processing Method: Cold Seal Adhesive, Inner Web Adhesive Lamination, Inner Web Extrusion Lamination, Outer Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing and Surface Print Unsupported

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brightness 90.0 %Whiteness Index
Water Vapor Transmission 0.0520 g/100 in²/day
@Temperature 23.0 °C
85% RH; ExxonMobil Method
 0.260 g/100 in²/day
@Temperature 38.0 °C
90% RH; ExxonMobil Method
Thickness 1.60 milExxonMobil Method
Coating Weight 19.6 lb/reamExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 160 %7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 65 %7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Modulus of Elasticity 247 ksiMD; ExxonMobil Method
 464 ksiTD; ExxonMobil Method
Coefficient of Friction 0.25Untreated Surface; ExxonMobil Method
 0.30Treated Surface; ExxonMobil Method
Seal Strength 410 g/in
@Pressure 0.276 MPa,
Temperature 140 °C
Otto Brugger, 0.2 sec; ExxonMobil Method
Film Tensile Strength at Break, MD 17400 psi7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 29000 psi7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 3.0 %
@Temperature 135 °C,
Time 432 sec
ExxonMobil Method
Shrinkage, TD 3.0 %
@Temperature 135 °C,
Time 432 sec
ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Gloss 55 %45°; ExxonMobil Method
Transmission, Visible 27 %ExxonMobil Method
 
Descriptive Properties
Heat Seal Range45°FUntreated/Treated, 36.3 psi, 0.2 sec
 54°FUntreated/Untreated, 36.3 psi, 0.2 sec
Yield22000 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ravago Manufacturing Americas Echo® RPPC 20/6 BK Polypropylene Copolymer
Phillips 66 COPYLENE® CH020-01 Polypropylene, Homopolymer, BOPP
ExxonMobil Oppalyte™ 60MH247 OPP Film
DuPont Teijin Films Mylar® RL32 Polyester Packaging Film, 100 Gauge
Borealis BorPURE™ RE450MO Polypropylene Random Copolymer

PEX99510 / 175746

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.