MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Wacker Wacker® P 300 Silicone Paste
Categories: Polymer; Thermoset; Silicone

Material Notes: Product description: WACKER® SILICONE PASTE P 300 is opaque, of medium to soft consistency and slightly thixotropic.

Properties: It has good electrical properties, i.e. insulating properties, dielectric constant and dielectric strength, as well as good adhesion to metals and ceramic materials. WACKER® SILICONE PASTE P 300 coated parts exhibit excellent water repellency, resulting in a certain degree of protection against corrosion. WACKER® SILICONE PASTE P 300 is a paste with similar properties like WACKER SILICONE PASTE P 250 but of softer consistency with an unworked penetration of 290 - 330 ¹/ ¹º mm. The low viscosity of the paste facilitates its use as an embedding compound, release agent or lubricant in some class.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³ISO 1183-1 A
Volatiles <= 3.5 %
@Temperature 200 °C,
Time 108000 sec
<= 3.5 %
@Temperature 392 °F,
Time 30.0 hour
FED-STD 791 M 321
 
Mechanical PropertiesMetricEnglishComments
Penetration 290 - 330290 - 330[1/10 mm], unworked; DIN ISO 2137
Penetration P(60), 1/10 mm 350350worked; DIN ISO 2137
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.1
@Frequency 50 Hz
3.1
@Frequency 50 Hz
IEC 60250
Dielectric Strength 20.0 kV/mm508 kV/inDIN 53481
Dissipation Factor 0.0070
@Frequency 50 Hz
0.0070
@Frequency 50 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Solidus -45.0 °C-49.0 °F
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Descriptive Properties
Appearancecolorless, opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9817 / 205346

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.