MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Thermal Ceramics Superwool 607 PM Board
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Superwool 607 PM boards are processed from a slurry consisting of Superwool bulk and organic binders. This board product is noted for its excellent surface finish, thickness uniformity and high insulating value at elevated temperatures.

Superwool provides stability and resistance to chemical attack. Exceptions include hydrofluoric acid, phosphoric acid and strong alkalis (i.e. NaOH, KOH). Superwool is unaffected by incidental spills of oil or water. Thermal and physical properties are restored after drying.

The non-wetting characteristics of the Superwool 607 PM Board composition make is an excellent alternative for molten aluminium contact.

Features:

  • Continuous temperature rating of 1832°F
  • Low thermal conductivity and heat storage
  • Very close thickness tolerance
  • Excellent surface finish and uniformity
  • Easily fabricated and die-cut
  • Applications:

  • Appliance and heat processing equipment insulation
  • Combustion chamber construction for domestic appliance construction
  • Heat shields
  • High temperature gaskets and seals
  • Back-up insulation to dense refractories
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.240 - 0.272 g/cc0.00867 - 0.00983 lb/in³
    Loss On Ignition 2.0 - 4.0 %2.0 - 4.0 %
     
    Mechanical PropertiesMetricEnglishComments
    Modulus of Rupture 0.00138 - 0.00172 GPa0.200 - 0.250 ksi
    Compressive Yield Strength 0.103 - 0.172 MPa14.9 - 24.9 psiat 5% deformation
     0.172 - 0.276 MPa24.9 - 40.0 psiat 10% deformation
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.0576 W/m-K
    @Temperature 260 °C
    0.400 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    ASTM C201
     0.0893 W/m-K
    @Temperature 538 °C
    0.620 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    ASTM C201
     0.143 W/m-K
    @Temperature 816 °C
    0.990 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    ASTM C201
     0.189 W/m-K
    @Temperature 982 °C
    1.31 BTU-in/hr-ft²-°F
    @Temperature 1800 °F
    ASTM C201
    Melting Point 1275 °C2327 °F
    Maximum Service Temperature, Air 1000 °C1832 °F
    Shrinkage 1.0 %
    @Temperature 982 °C,
    Time 86400 sec
    1.0 %
    @Temperature 1800 °F,
    Time 24.0 hour
     
    Component Elements PropertiesMetricEnglishComments
    CaO 27 %27 %
    MgO 5.0 %5.0 %
    Other 1.0 %1.0 %
    SiO2 67 %67 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Zircar Zirconia ZYF-A2.13 Zirconia Felt Insulation
    Thermal Ceramics Kaowool 3000 High Temperature Board
    Thermal Ceramics 2100 RPC Shapes
    Schott ZERODUR® K20 Glass Ceramic
    Cotronics Resbond™ 919 High Temperature Ceramic Adhesive, High Resistance

    CTHERM291 / 2611

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.