MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Industeel FORA 500 500 HB Wear Resistant Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Medium Carbon Steel

Material Notes: Description: FORA 500 is a water quenched martensitic steel, with a 500HB (51.5 HRC), typical hardness, resistant to very severe abrasion wear. Thanks to its mechanical properties, good toughness, high hardness and strength, FORA 500 steel can be used wherever a sliding wear resistance is required and where 400 HB steels do not provide sufficiently long service life. Compared to conventional steels, such as S355, FORA 500 offers a real improvement on the life time of equipment, up to 5 times longer and consequently allows a significant reduction in the design thickness. FORA 500 steel is particularly suitable for applications such as quarries, construction equipment, mines, cement plants, the iron and steel industry, etc.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 460 - 540Typical
Hardness, Rockwell C 49 - 54Typical
Tensile Strength, Ultimate 1700 MPaTypical
Tensile Strength, Yield 1350 MPa
@Strain 0.2 %
Typical
Elongation at Break 10 %Typical
Charpy Impact 30.0 J
@Temperature -20.0 °C
Typical
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.26 %
Chromium, Cr 1.9 %
Iron, Fe 96.485 - 96.51 %As remainder
Manganese, Mn 1.3 %
Molybdenum, Mo 0.030 %
Phosphorus, P <= 0.020 %
Sulfur, S <= 0.0050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Industeel FORA 400 Wear Resistant Steel, 400 HB
ThyssenKrupp PAS 355 Structural Steel for Cold Forming
ThyssenKrupp XABO® 355 Structural Steel
ASTM A572 Steel, grade 42
Industeel CREUSABRO® 8000 High Performance Wear Resistant Steel

NINDUST61 / 17599

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.