MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elix Polymers ELIX™ 290 G SAN copolymer
Categories: Polymer; Thermoplastic; SAN Polymer

Material Notes: High Molecular Weight SAN copolymer.

Typical applications:

  • Used to improve dimensional and thermal stability in PVC extruded applications
  • Can be blended with High Rubber Modifiers (ELIX™ 100 series) to manufacture or modify properties profile of ABS resin
Major benefits:
  • Improves melt strength and melt stability in PVC compositions and ABS resin
  • Allows superior dynamic loading performance for ABS resin
Chemical composition: Styrene-Acrylonitrile Copolymer

Physical form: Transparent to slightly yellow pellets

Information provided by Elix Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 9.0 - 12 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Descriptive Properties
Base color<8020% solution in DMF, DIN 6271
Content<750 ppmResidual Styrene
 23-24.5%Acrylonitrile

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elix Polymers Elix™ 260 G SAN Polymer Modifier
Elix Polymers Elix™ 280 G SAN Polymer Modifier
Elix Polymers Elix™ 230 G SAN Polymer Modifier
Elix Polymers ELIX ABS P2M-AT Acrylonitrile Butadiene Styrene (ABS), High Impact Strength
Elix Polymers ELIX ABS P2H-AT Acrylonitrile Butadiene Styrene (ABS)

PELIX044 / 183359

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.