MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Wacker ELASTOSIL® R PLUS 4285/30 Solid Silicone Rubber-Batch Grade
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: ELASTOSIL® R PLUS 4285/30 is intended for fabrication of molded articles that afford high elongation and low tension set, like catheter balloons.

Properties: ELASTOSIL® R PLUS 4285/30 HCR silicone rubber is an addition-curing, two part compound. The vulcanizates show excellent transparency and good to very good mechanical properties. Properly postcured vulcanizates of ELASTOSIL® R PLUS 4285/30 should comply with BfR and FDA food contact regulations. The material should also pass USP XXIII Class VI and ISO 10993 standards.

Information provided by Wacker.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30ASTM D2240
Tensile Strength 7.00 MPaASTM D412
Elongation at Break 900 %ASTM D412
Tear Strength 200 plidie B; ASTM D 624
Tensile Set 2.0 - 3.0 %3d@RT, 400%; WSTM 1309
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
AppearanceTranslucentWSTM 1279

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Elastosil® LR 3003/03 A/B Liquid Silicone Rubber
Wacker ELASTOSIL® R plus 4105/60 Solid Silicone Rubber-Batch Grade
ATG s.r.l. AU-EU Polyurethane Rubber
Fluorosilicone Rubber (FMQ, FVMQ, FSi)
Overview of materials for Nylon 6, Film Grade

PWACK9932 / 197531

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.