MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Tin Brass, Copper Alloy, UNS C43000, H08 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: Spring

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Butt Weld, Capacity for Being Hot Formed; Fair Suitability – Spot Weld

Common Fabrication Processes: Bending; Blanking; Coining; Drawing; Forming; Heading; Upsetting

Typical Uses: Sash Chain; Weather Stripping; Pen Clips; Electrical Connectors; Fuse Clips; Switches; Platers Bars and Cores; Springs; Timer Contact Blades – Flexing; Wire Supports in Optical Work

Applicable Specifications: Bar – ASTM B591; Plate – ASTM B591; Sheet – ASTM B591; Strip – ASTM B591

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.75 g/cc0.316 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 9191
Hardness, Rockwell 30T 7777
Tensile Strength 648 MPa94000 psi
Tensile Strength, Yield 496 MPa72000 psi0.5% Ext
Elongation at Break 4.0 %4.0 %
Tensile Modulus 110 GPa16000 ksihard tempers
Machinability 30 %30 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000640 ohm-cm0.00000640 ohm-cm27% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.4 µm/m-°C
@Temperature 20.0 - 100 °C
10.2 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 9.94 W/m-K69.0 BTU-in/hr-ft²-°F
Melting Point 1000 - 1025 °C1832 - 1877 °F
Solidus 1000 °C1832 °F
Liquidus 1025 °C1877 °F
Annealing Point 427 - 704 °C800 - 1300 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 790.6 - 840.6 °C1455 - 1545 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 84 - 87 %84 - 87 %
Iron, Fe <= 0.050 %<= 0.050 %
Lead, Pb <= 0.090 %<= 0.090 %
Tin, Sn 1.7 - 2.7 %1.7 - 2.7 %
Zinc, Zn 10.2 - 14.3 %10.2 - 14.3 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC43000y1 / 291965

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.