MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Radici RENYCLE® S T203K 3030 BK Nylon 6, Heat Stabilized, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized

Material Notes: Description: Partially recycled PA6 injection molding grade. Toughened. Heat stabilized. Black color. This material has been developed to reduce its environmental impact compared to first-choice grades, through the recovery of post-consumer (end-of-life) components previously classified as waste.

Processing: Injection Molding

Delivery Form: Granules

Additives: Release agent

Special Characteristics: High impact or impact modified, Heat stabilized or stable to heat

Sustainability: Pre-consumer Recycling

Industries: Automotive, Consumer Industry Goods, Transportation

Regional Availability: Europe

Information provided by Radici Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.014 cm/cm0.014 in/inMelt Temp/Mold Temp/Cavity Pressure: 250/80/60; ISO 294-4
Linear Mold Shrinkage, Transverse 0.016 cm/cm0.016 in/inMelt Temp/Mold Temp/Cavity Pressure: 250/80/60; ISO 294-4
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 250 °C
20 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 35.0 MPa5080 psi50 mm/min; ISO 527-2/1A
Elongation at Yield 230 %230 %50 mm/min; ISO 527-2/1A
Tensile Modulus 0.850 GPa123 ksi1mm/min; ISO 527-2/1A
Flexural Strength 30.0 MPa4350 psi2mm/min; ISO 178
Flexural Modulus 0.720 GPa104 ksi2mm/min; ISO 178
Charpy Impact, Notched 9.00 J/cm²42.8 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 11357-1/-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 280 °C464 - 536 °F
Mold Temperature 70.0 - 80.0 °C158 - 176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADICI041 / 313542

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.