MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Reade Advanced Materials Gadolinium Zirconate Powder (Gd2Zr2O7)
Categories: Ceramic; Oxide

Material Notes: Low thermal conductivity oxide used as a thermal barrier coating and for corrosion resistance. Gadolinium zirconate is a very radiation-resistant material.

Information provided by Reade Advanced Materials.

Key Words: Gd2Zr2O7, GZO
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.32 g/cc0.228 lb/in³
Molecular Weight 608.944 g/mol608.944 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 12001200kgf/mm²
 
Thermal PropertiesMetricEnglishComments
Melting Point 2570 °C4660 °F
 
Descriptive Properties
CAS Number11073-79-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Piezo Kinetics PKI 532 Lead Zirconate Titanate Piezoelectric
Piezo Kinetics PKI 809 Navy Type III Lead Zirconate Titanate Piezoelectric
Piezo Kinetics PKI 804 Navy Type III Lead Zirconate Titanate Piezoelectric
Piezo Kinetics PKI 556 Lead Zirconate Titanate Piezoelectric
Piezo Kinetics PKI 552 Lead Zirconate Titanate Piezoelectric

CREADE035 / 199558

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.