MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Austin Novel Materials Texalan® 395A Polyester-based TPU
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Good abrasion resistance, tensile strength, oil resistance; can be used in injection or extrusion.

Information from Dawnentech

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 - 1.23 g/cc0.0430 - 0.0444 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 92 - 9892 - 98ISO 7619
Tensile Strength >= 42.0 MPa>= 6090 psiISO 37
Tensile Stress at Strain  >= 9.00 MPa
@Strain 100 %
>= 1310 psi
@Strain 100 %
ISO 37
 >= 21.0 MPa
@Strain 300 %
>= 3050 psi
@Strain 300 %
ISO 37
Elongation at Yield >= 450 %>= 450 %ISO 37
Tear Strength >= 105 kN/m>= 599 pliISO 34
K Factor (Wear Factor) <= 55<= 55[mm3]; ISO 4649
Compression Set <= 50 %
@Temperature 70.0 °C
<= 50 %
@Temperature 158 °F
ISO 815

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Austin Novel Materials Texalan® 390A Polyester-based TPU
Austin Novel Materials Texalan® 295A Polyester-based TPU
Austin Novel Materials Texalan® 290A Polyester-based TPU
Austin Novel Materials Texalan® 795A PCL TPU
Austin Novel Materials Texalan® 790A PCL TPU

PDAWNE015 / 123249

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.