MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Phillips 66 Triton® OG SS AGMA Grade 14R
Categories: Fluid; Lubricant

Material Notes: Phillips 66® Triton® OG SS is a high-performance, semi-synthetic gear lubricant specifically developed to meet the demands of heavily loaded, slow moving gears and bearings. It is recommended primarily for the lubrication and cushioning of open and semi-enclosed gear drives found in mills and kilns. Triton OG SS is formulated with a carefully selected combination of synthetic base stocks, high-viscosity mineral oils and extreme-pressure additives to minimize wear in large roller and thrust bearings and to protect heavily loaded, low-speed gears under boundary lubrication conditions. The use of synthetic base stocks produces a lubricant with high viscosity index that allows for good pumpability at lower temperatures while maintaining excellent film thickness at higher temperatures. Triton OG SS does not contain heavy metals, bitumen or solid additives.

Applications:

  • Large roller and thrust bearings in sugar mills
  • Open and semi-enclosed gear drives in rotary kilns and mills found in cement, limestone and gypsum production
  • Slow-speed, heavily loaded plain and rolling contact bearings
Triton OG SS meets the requirements of the following industry specification:
  • ANSI/AGMA Standard 9005-E02
Features/Benefits:
  • Excellent adhesion to metal surfaces
  • Extreme-pressure protection
  • High film strength reduces the tendency for fluid “squeeze out” in highly loaded and slowly rotating gears and bearings
  • Good resistance to water washout
  • Excellent pumpability at low ambient temperatures
  • Does not contain heavy metals, bitumen or solid additives
  • Solvent-free formulation
  • Amber-colored product
  • Suitable for use in existing lubricant spray systems, allowing for easy conversion from lubricants containing bitumen

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.899 g/cc0.899 g/cc
Density 0.899 g/cc0.0325 lb/in³
Viscosity Measurement 185185Index
Kinematic Viscosity at 40°C (104°F) 15834 cSt15834 cSt
Kinematic Viscosity at 100°C (212°F) 551 cSt551 cSt
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 400 kg882 lb (mass)ASTM D2596
Four Ball Wear 0.490 mm0.0193 inScar Diameter; ASTM D4172B
Timken Test 29500 g65.0 lbASTM D2782
 
Thermal PropertiesMetricEnglishComments
Pour Point -13.0 °C8.60 °F
Flash Point 210 °C410 °FCOC
 
Descriptive Properties
ColorAmber
Copper Corrosion1bASTM D130

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5443 / 198696

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.