MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Röchling SUSTAPEEK® MOD
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: Product characteristics:
  • High rigidity
  • Excellent sliding and abrasion behavior
  • Good dimensional stability
Product applications:
  • Medical engineering
  • Materials handling industry
  • Electrical industry

Information provided by Röchling.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³DIN EN ISO 1183-1
Water Absorption 0.20 %0.20 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585DIN EN ISO 868
Tensile Strength, Yield 75.0 MPa10900 psiDIN EN ISO 527
Elongation at Break 4.0 %4.0 %DIN EN ISO 527
Modulus of Elasticity 4.90 GPa711 ksiDIN EN ISO 527
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²DIN EN ISO 179
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 µm/m-°C16.7 µin/in-°FDIN 53752
Thermal Conductivity 0.240 W/m-K1.67 BTU-in/hr-ft²-°FDIN 52612-1
Melting Point 343 °C649 °FISO 11357-3
Maximum Service Temperature, Air 250 °C482 °Flong term
 310 °C590 °Fshort term
Deflection Temperature at 1.8 MPa (264 psi) 293 °C559 °FDIN EN ISO 75
Minimum Service Temperature, Air -30.0 °C-22.0 °F
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 6.00 mm
V-0
@Thickness 0.236 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röchling SUSTAPEEK® PEEK
Röchling SUSTAPEEK® PEEK
Röchling SUSTAPEEK® MOD ESD 90
Röchling SUSTAPEEK® MG natural Medical Grade PEEK
Röchling SUSTAPEEK® GLD 140 FG natural PEEK

PROCH9330 / 233032

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.