TABOREN-PC 69 G 40 is a compound based on polypropylene copolymer filled with 40% of short glass fiber, stabilized with a high antioxidant package. It is designed for injection molding technology and used in many industrial fields with stress put on excellent processability and good surface performance.Information provided by Silon US LLC. |