MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eastman Eastman Advantis™ 515-2 40A adhesion promoter
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Eastman Advantis™ 515-2 40A adhesion promoter (40% in Aromatic 100) is a liquid at room temperature. If the solution gels due to storage at low temperatures, it can be re-liquified by warming to 38°C with agitation. Solutions of Eastman Advantis 515-2 40A adhesion promoter (as supplied) can easily be reduced with xylene, toluene, selected ketones, and ester solvents. Advantis 515-2 40A has good heat resistance and is compatible with a variety of resins. It combines with the resins to give clear solutions and deposit clear films. Advantis™ 515- 2 40A also has excellent adhesion to polypropylene and good-to-excellent adhesion to many other substrates. Advantis 515-2 40A not only adheres to a variety of substrates, but when added to coatings and inks it improves their adhesion to these substrates.

Applications

  • Auto omen
  • Commercial printing inks
  • General industrial coatings
  • Graphic arts
  • Protective coatings

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³
 1.04 - 1.09 g/cc0.0376 - 0.0394 lb/in³Solid CPO
 
Thermal PropertiesMetricEnglishComments
Flash Point 41.0 °C106 °FTag Closed Cup
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 7.007.00
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 26.0 - 32.0 %26.0 - 32.0 %
 
Descriptive Properties
Content<0.1 %Isopropylbenzene (Cumene)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM4010 / 323633

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.