Product data demonstrates the effect of the Novakup® (lamellar quartz surface treated with A-1100) filler. A separate entry demonstrates the effect of untreated Novacite® filler in nylon. The specific nylon used is Huels Nylon 12 L-1901, granulated natural, L-809-0001-0718.Information provided by Malvern Minerals Company. |