MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Teresstic 77
Categories: Fluid; Lubricant

Material Notes: TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERESSTIC oils are formulated with carefully selected base stocks and highly effective additives, including oxidation and rust inhibitors and anti-foam agents. The TERESSTIC line of premium circulating oils consists of nine viscosity grades. Eight of these grades are blended to viscosity values that conform to the International Organization for Standardization (ISO) viscosity classification system. TERESSTIC 77 is an intermediate grade between ISO viscosity grades 68 and 100.

TERESSTIC oils are the primary recommendation for applications that require clean, dependable lubrication for extended service periods – often for years. They effectively resist high temperatures, prevent rust, and shed entrained water and air. Because the quality of TERESSTIC oils is especially apparent at sustained high temperatures and other adverse operating conditions, they are the prime lubricant recommendation for mild duty industrial gas turbines that require mineral lubricating oils. In addition, TERESSTIC oils give outstanding performance in hydraulic systems, circulating lubrication systems, gear cases, bearings, and other industrial units, where an RandO lubricant is required, for which long trouble-free service is required. Their high flash points suit TERESSTIC oils for use as heat transfer fluids in open systems. TERESSTIC 32 and 46 – These grades are formulated for applications where a premium quality grade 32 or 46 lubricant is required, but where service conditions are not severe enough to require the super-premium qualities of TERESSTIC GT 32 and 46. TERESSTIC 32 and 46 are of the same high quality as the heavier TERESSTIC grades and provide excellent performance in mild duty applications. Contamination of TERESSTIC oils with other products such as detergent motor oils may substantially impair their quality and could lead to operational problems such as foaming, filter plugging and sludge formation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.881 g/cc
@Temperature 15.6 °C
0.881 g/cc
@Temperature 60.1 °F
ASTM D1298
API Gravity 29.1 °29.1 °15.6°C; ASTM D1298
Viscosity Measurement 9797Index; ASTM D2270
Saybolt Viscosity at 100°F 396 SUS396 SUS
Saybolt Viscosity at 210°F 57.7 SUS57.7 SUS
Kinematic Viscosity at 40°C (104°F) 77 cSt77 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 9.3 cSt9.3 cStASTM D445
Oxidative Stability 2000 hour2000 hourTurbine Oil Stability Test (TOST); ASTM D943
 
Thermal PropertiesMetricEnglishComments
Pour Point -12.0 °C10.4 °FASTM D97
Flash Point 250 °C482 °FASTM D92
 
Descriptive Properties
Copper Strip Corrosion1B3 hrs @ 100°C
Demulsibility Time (min)10to 3 mL emulsion @ 54°C
Foam Sequence I, ASTM D9620/0
Foam Sequence II, ASTM D89330/0
Foam Sequence III, ASTM D8930/0
Neutralization Number, ASTM D9740.06
Rust Prevention, Distilled WaterpassASTM D665A
Rust Prevention, Synthetic Sea WaterpassASTM D665B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WEXXON142 / 75567

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.