MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC LNP™ THERMOCOMP™ Compound RF008 Polyamide 66 (Nylon 66) (Americas)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: LNP THERMOCOMP RF008 compound is based on Nylon 6/6 resin containing 40% glass fiber.

Features: High Stiffness,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc1.50 g/ccASTM D792
Density 1.48 g/cc0.0535 lb/in³ASTM D792
Moisture Absorption 0.150 - 0.250 %0.150 - 0.250 %Injection Molding
 0.660 %0.660 %23°C/50% RH/24 hrs; ASTM D570
 1.00 %1.00 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.010 - 0.030 cm/cm0.010 - 0.030 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 210 MPa30500 psi5 mm/min; ASTM D638
 232 MPa33600 psi5 mm/min; ISO 527
Tensile Strength, Yield 230 MPa33400 psi5 mm/min; ASTM D638
 232 MPa33600 psi5 mm/min; ISO 527
Elongation at Break 2.9 %2.9 %5 mm/min; ASTM D638
 2.9 %2.9 %5 mm/min; ISO 527
Elongation at Yield 2.8 %2.8 %5 mm/min; ASTM D638
 2.9 %2.9 %5 mm/min; ISO 527
Tensile Modulus 13.9 GPa2020 ksi5 mm/min; ASTM D638
 14.06 GPa2039 ksi1 mm/min; ISO 527
Flexural Strength 229 MPa33200 psiISO 178
 337 MPa48900 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
 338 MPa49000 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 11.17 GPa1620 ksi2 mm/min; ISO 178
 12.4 GPa1800 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 166 J122 ft-lbASTM D256
Izod Impact, Unnotched 13.2 J/cm24.7 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 16.0 kJ/m²7.61 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 86.0 kJ/m²40.9 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 18.0 J13.3 ft-lbASTM D3763
Impact Test 4.00 J2.95 ft-lbMultiaxial Impact; ISO 6603
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 32.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
17.8 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 62.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
34.4 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 259 °C498 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 260 °C
@Thickness 3.20 mm
500 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 242 °C468 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 253 °C
@Thickness 3.20 mm
487 °F
@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 280 - 295 °C536 - 563 °F
Zone 3 295 - 305 °C563 - 581 °F
Melt Temperature 280 - 305 °C536 - 581 °FInjection Molding
Mold Temperature 95.0 - 110 °C203 - 230 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81880 / 289827

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.