MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Malvern Minerals Thermoplastic Polyester with Novakup® 1250 Silane-Treated Quartz Filler
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Product data demonstrates the effect of the Novakup® (lamellar quartz surface treated with 0.5% A-1100) filler. A separate entry demonstrates the effect of untreated Novacite® filler in thermoplastic polyester. The specific thermoplastic polyester is Celanex J-105.

Information provided by Malvern Minerals Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 42.1 MPa6100 psiafter 16 hours in 50°C water
 46.9 MPa6800 psiinitial
Flexural Strength 95.8 MPa13900 psiafter 16 hours in 50°C water
 98.6 MPa14300 psiinitial
Flexural Modulus 5.58 GPa810 ksiinitial
 5.58 GPa810 ksiafter 16 hours in 50°C water
Izod Impact, Unnotched 1.39 J/cm2.60 ft-lb/in
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 125 °C257 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mocom (ALBIS) ALTECH® PA66 A 1000/517.01 IM Nylon 66
Taiwan Sheen Soon Sheenthane® AH-782 TPU for Hotmelt Adhesive
SunChemical Gwent C2010517D4 Carbon/Graphite Ink
Silane, SiH4
RTP Company PermaStat® 1100A EG  Polyethylene Terephthalate Glycol Modified (PETG) Anti-static - Extrusion Grade

PMALV967 / 149103

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.