MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution Absolan® 25GF30%
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Molded, Glass Reinforced

Material Notes: Absolan® 25GF30% is glass filled grade with medium flow, high rigidity injection molding grade. High Rigidity, Good dimensional stability, Low mold shrinkage. Applications: Air conditioner blower, Cross flow fans, Electrical capacitors

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 7.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 95.0 MPaISO 527
Tensile Modulus 12000 MPaISO 527
Flexural Strength >= 150 MPaISO 178
Flexural Modulus 9000 MPaISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature 23.0 °C
1/4" bar, 0.01" Notch Radius
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 101 °Cannealed 4 hours at 80°C; ISO 75
Vicat Softening Point >= 109 °C
@Load 1.02 kg
B/2 120C/H; ASTM D 1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUPOS GP2305A SAN+GF30%, General Purpose
Polyram RamShine PW300G7 SAN, 35% Glass Fiber
Polykemi AB POLYsan FL100 F35 SAN, Glass Fiber-Reinforced
Lotte Advanced Materials Starex® GR-5020T SAN, 20% Glass Filled
Ineos ABS Lustran® SAN GF30 Glass Fiber Reinforced

PSTYR9858 / 216085

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.