MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta NP130HF Epoxy Glass Laminate Sheet, NEMA FR-4
Categories: Polymer; Thermoset; Epoxy

Material Notes: NP130HF is a woven glass fabric composite combined with epoxy resin system, which is engineered to provide better physical properties than standard NEMA FR-4. It is significantly more dimensionally stable than NP130 or NP510A because of its low resin content. The main application for NP130HF is for “bed-of-nails” probe boards used for printed circuit board testing, and other structural applications.

Information provided by Norplex-Micarta

Key Words: Glass Fiber, Epoxy, Micarta, NEMA FR-4, ASTM D709 Type IV Grade FR-4, MIL-I-24768/27 GEE-F, IPC 4101/21
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.95 g/cc
@Thickness 12.7 mm
ASTM D792
Moisture Absorption 0.130 %
@Thickness 1.57 mm
ASTM D570 Condition A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 110
@Thickness 6.35 mm
ASTM D785
Tensile Strength 65000 psi
@Thickness 3.17 mm
CrossWise; ASTM D638 Condition A
 70000 psi
@Thickness 3.17 mm
LengthWise; ASTM D638 Condition A
Flexural Strength 70000 psi
@Thickness 1.57 mm
CrossWise; ASTM D790 Condition A
 85000 psi
@Thickness 1.57 mm
LengthWise; ASTM D790 Condition A
Flexural Modulus 3000 ksi
@Thickness 1.57 mm
CrossWise; ASTM D790 Condition A
 3700 ksi
@Thickness 1.57 mm
LengthWise; ASTM D790 Condition A
Compressive Strength 71000 psi
@Thickness 12.7 mm
Flatwise; ASTM D695 Condition A
Shear Strength 23000 psi
@Thickness 1.57 mm
perpendicular; ASTM D732 Condition A
Izod Impact, Unnotched 9.00 ft-lb/in
@Thickness 12.7 mm
CrossWise; ASTM D256 Condition E-48/50
 13.0 ft-lb/in
@Thickness 12.7 mm
LengthWise; ASTM D256 Condition E-48/50
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.8
@Thickness 1.57 mm,
Frequency 1e+6 Hz
ASTM D150 Condition D-24/23
Dielectric Strength 700 V/mil
@Thickness 1.57 mm
ASTM D149 Condition D-48/50
 900 V/mil
@Thickness 1.57 mm
ASTM D149 Condition A
Dielectric Breakdown 65000 V
@Thickness 1.57 mm
ASTM D149 Condition D-48/50
 70000 V
@Thickness 1.57 mm
ASTM D149 Condition A
Dissipation Factor 0.022
@Thickness 1.57 mm,
Frequency 1e+6 Hz
ASTM D150 Condition D-24/23
Arc Resistance 75 sec
@Thickness 3.17 mm
ASTM D495 Conition A
Comparative Tracking Index 150 V
@Thickness 3.17 mm
ASTM D3638
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 14.7 µm/m-°C
@Thickness 3.17 mm
IPC-TM 650-2.4.24
CTE, linear, Transverse to Flow 13.7 µm/m-°C
@Thickness 3.17 mm
IPC-TM 650-2.4.24
Transformation Temperature, Tg 130 °C
@Thickness 12.7 mm
DMA
UL RTI, Electrical 130 °CUL Bulletin 746b
UL RTI, Mechanical with Impact 140 °CUL Bulletin 746b
Flammability, UL94 V-0
@Thickness 1.57 mm
 
Descriptive Properties
Bonding Strength2500[lb]; 0.5"; ASTM D229 Condition D-48/50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Norplex-Micarta NP130 Epoxy Glass Laminate Sheet, NEMA FR-4
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
G-10 Fiberglass Epoxy Laminate Sheet
Norplex-Micarta MC511A Epoxy Glass Laminate Sheet, NEMA G-11
Norplex-Micarta NP500A Epoxy Glass Laminate Sheet, NEMA G-10

PNORPM050 / 192807

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.