MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Solvay DAPCO™ 3100FR Paste Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: DAPCO™ 3100FR is a two-component, self-extinguishing, room temperature curing, epoxy-based, 100% solids, structural adhesive designed for various bonding applications. It maintains good strength retention up to 400°F (204°C).

Features & Benefits:

  • Thixotropic flow properties
  • 100% solids content
  • Room temperature cure
  • Room temperature storage
  • Meets FAR 25.853
Applications: DAPCO 3100FR is used in bonding and liquid shim applications where high temperature exposure is required.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³Part B
 1.23 g/cc0.0444 lb/in³Mixed
 1.37 g/cc0.0495 lb/in³Part A
Solids Content 100 %100 %Part A
 100 %100 %Part B
 100 %100 %Mixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 70 - 8070 - 80
Adhesive Bond Strength  4.14 MPa
@Temperature 204 °C
600 psi
@Temperature 399 °F
Shear, Aluminum (2024-T3) clad, FPL etch + PAA (phosphoric acid anodized)
 7.970 MPa
@Temperature 177 °C
1156 psi
@Temperature 351 °F
Shear, Aluminum (2024-T3) clad, FPL etch + PAA (phosphoric acid anodized)
 27.28 MPa
@Temperature 24.0 °C
3957 psi
@Temperature 75.2 °F
Shear, Aluminum (2024-T3) clad, FPL etch + PAA (phosphoric acid anodized)
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °Fgood strength retention
 
Descriptive Properties
ColorAmberPart A
 CreamPart B
 CreamMixed
Mix Ratio100:23

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCYTED023 / 180325

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.