MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

BASF Ultramid® A 218G V33 Black 41N Nylon 66, 33% Glass Fiber Reinforced, Heat Stabilized, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Product Description: Ultramid® A 218G V33 Black 41N is a polyamide 66, reinforced with 33% of glass fiber, for injection molding. This grade has been specially designed to improve its resistance to automotive cooling liquids, increasing lifetime of parts in permanent contact with such liquids.

Availability: North America

Filler/Reinforcement: Glass Fiber, 33% Filler by Weight

Features: Good Flow; Good Mold Release; Hydrolysis Resistant; Outstanding Surface Finish

Use: Automotive Applications; General Purpose

RoSH Compliance: RoSH Compliant

Appearance: Black

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA66-GF33

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³ISO 1183
Water Absorption 1.7 %1.7 %Equilibrium, 50% RH; ISO 62
 0.78 %
@Time 86400 sec
0.78 %
@Time 24.0 hour
ISO 62
Water Absorption at Saturation 5.3 %5.3 %ISO 62
Maximum Moisture Content 0.150.15
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 185 MPa26800 psiISO 527-2
 190 MPa27600 psiASTM D638
Elongation at Break 3.2 %3.2 %ISO 527-2
 3.4 %3.4 %ASTM D638
Tensile Modulus 11.3 GPa1640 ksiISO 527-1
Flexural Strength 264 MPa38300 psiISO 178
Flexural Modulus 8.69 GPa1260 ksiASTM D790
 9.93 GPa1440 ksiISO 178
Izod Impact, Notched (ISO) 10.1 kJ/m²4.80 ft-lb/in²ISO 180/A
Charpy Impact Unnotched 8.40 J/cm²40.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²5.70 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 262 °C504 °FISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FUnannealed; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 270 - 280 °C518 - 536 °F
Middle Barrel Temperature 275 - 285 °C527 - 545 °F
Front Barrel Temperature 280 - 290 °C536 - 554 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2086 / 310779

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.