Injection molding grade with exceptionally good flow, for Digital Versatile Discs (DVD). Information provided by Bayer. As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation. |