MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
RAMPF RAKU® TOOL IE-3252 Polyurethane, polyether based elastomer
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Elastic Polyether system

Key Properties:

  • Excellent physical properties after RT cure
  • Free of mercury, MOCA or TDI
  • Ideal for color matching due to its neutral color
Applications:
  • For hand-batch processing
Cure 1: 24 hours at 77°F + 16 hours at 150°F
Cure 2: 7 days at 77°F

Information provided by © RAMPF Tooling Solutions GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/ccHardener; ASTM D-792
 1.09 g/ccCure 1; ASTM D-792
 1.09 g/ccCure 2; ASTM D-792
 1.13 g/ccResin; ASTM D-792
Viscosity 75 cPResin; ASTM D-2393
 800 cPMix; ASTM D-2393
 1400 cPHardener; ASTM D-2393
Linear Mold Shrinkage 0.0010 - 0.0040 in/inCure 1; ASTM D-2566
 0.0010 - 0.0040 in/inCure 2; ASTM D-2566
Storage Temperature 15.0 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 45 - 55Cure 1; ASTM D-2240
 45 - 55Cure 2; ASTM D-2240
Tensile Strength 900 psiCure 1; ASTM D-638
 1100 psiCure 2; ASTM D-638
Elongation at Break 520 %Cure 1; ASTM D-638
 520 %Cure 2; ASTM D-638
Tear Strength 90.0 pliCure 2; ASTM D-624
 120 pliCure 1; ASTM D-624
 
Processing PropertiesOriginal ValueComments
Cure Time 12.0 - 20.0 hourMix, Demold time
Gel Time 20.0 - 30.0 minMix
 
Descriptive Properties
AspectOff-whiteCure 1
 Off-whiteCure 2
Mix Ratio38:100Resin: Hardener, Volume
 40:100Resin: Hardener, Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRAMPF025 / 317625

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.