MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Akrochem HRJ-11331/R7522E Resin
Categories: Polymer; Thermoplastic

Material Notes: Product Description: HRJ-11331/R7522E is an oil-soluble phenolic resin made from para-tertiary butylphenol and formaldehyde that contains reactive methylol groups. This resin is most widely used in the formulation of polychloroprene contact cements that exhibit very high temperature performance and resistance to phasing.

Applications: HRJ-11331/R7522E is extensively employed in the preparation of general purpose and heat-activating pholychloroprene cements. It can also be used in formulating adhesives with NBR, SBR, natural and reclaimed rubbers. In polychloroprene adhesives, HRJ-11331/R7522E increases high temperature performance; increases the specific adhesion of the adhesive film to metal and glass, and increases cohesive strength of the adhesive film itself. HRJ-11331/R7522E is completely compatible with nitrile and polychloroprene rubbers. It has a compatibility limit of approximately 25 parts by weight in combination with 100 parts by weight of SBR, natural, and reclaimed rubber.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
 
Thermal PropertiesOriginal ValueComments
Melting Point 200 - 220 °CCapillary
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 1.0 - 7.064% in Toluene
 
Descriptive Properties
AppearanceFlake
Content10-14%Methylol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH408 / 315326

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.