MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

SABIC NORYL GTX GTX989 PPE+PA (Americas)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted body panels and fenders in particular. This material combines impact performance with conductivity for electro-static painting in an unique way.

Information provided by SABIC Innovative Plastics for the Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D 792
Density 1.08 g/cc0.0390 lb/in³ISO 1183
Moisture Absorption 1.20 %
@Temperature 23.0 °C
1.20 %
@Temperature 73.4 °F
50% RH; ISO 62
Water Absorption at Saturation 4.2 %
@Temperature 23.0 °C
4.2 %
@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage, Flow 0.012 - 0.016 cm/cm
@Thickness 3.20 mm
0.012 - 0.016 in/in
@Thickness 0.126 in
SABIC Method
Melt Flow  16 g/10 min
@Load 5.00 kg,
Temperature 280 °C
16 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D 1238
 19 g/10 min
@Load 5.00 kg,
Temperature 280 °C
19 g/10 min
@Load 11.0 lb,
Temperature 536 °F
cm^3/10 min Melt Volume Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 55.0 MPa7980 psi50 mm/min; ISO 527
 60.0 MPa8700 psiType I, 50 mm/min; ASTM D 638
Tensile Strength, Yield 60.0 MPa8700 psi50 mm/min; ISO 527
 65.0 MPa9430 psiType I, 50 mm/min; ASTM D 638
Elongation at Break 40 %40 %50 mm/min; ISO 527
 45 %45 %Type I, 50 mm/min; ASTM D 638
Elongation at Yield 5.0 %5.0 %50 mm/min; ISO 527
 5.0 %5.0 %Type I, 50 mm/min; ASTM D 638
Tensile Modulus 2.30 GPa334 ksi1 mm/min; ISO 527
 2.35 GPa341 ksi50 mm/min; ASTM D 638
Flexural Yield Strength 90.0 MPa13100 psi2 mm/min; ISO 178
 95.0 MPa13800 psi1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 2.30 GPa334 ksi2 mm/min; ISO 178
 2.45 GPa355 ksi1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched  1.80 J/cm
@Temperature -30.0 °C
3.37 ft-lb/in
@Temperature -22.0 °F
ASTM D 256
 2.40 J/cm
@Temperature 23.0 °C
4.50 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
Izod Impact, Notched (ISO)  15.0 kJ/m²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
 22.0 kJ/m²
@Temperature 23.0 °C
10.5 ft-lb/in²
@Temperature 73.4 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched  1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
 2.20 J/cm²
@Temperature 23.0 °C
10.5 ft-lb/in²
@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
Instrumented Impact Total Energy 60.0 J
@Temperature 23.0 °C
44.3 ft-lb
@Temperature 73.4 °F
ASTM D 3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1000 - 10000 ohm-cm1000 - 10000 ohm-cmSABIC Method
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  85.0 µm/m-°C
@Temperature -40.0 - 60.0 °C
47.2 µin/in-°F
@Temperature -40.0 - 140 °F
ASTM E 831
 90.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow  85.0 µm/m-°C
@Temperature -40.0 - 60.0 °C
47.2 µin/in-°F
@Temperature -40.0 - 140 °F
ASTM E 831
 90.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 190 °C374 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 190 °C
@Thickness 3.20 mm
374 °F
@Thickness 0.126 in
unannealed; ASTM D 648
Vicat Softening Point 195 °C383 °FRate B/50; ASTM D 1525
 195 °C383 °FRate B/50; ISO 306
 200 °C392 °FRate B/120; ISO 306

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® T95 MF Polycarbonate + ABS, Mineral Filled

PSABI47357 / 188442

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.