45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength Amodel® A-1145 HS LZT is an NIR laser transmissive, 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep resistance and low moisture absorption are also characteristic of this resin. This grade is designed to be paired with other Amodel® black grades for black-on-black laser welding applications. - Black: Amodel® A-1145 HS LZT BK 979 Applications: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Connectors; Housings; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools; Valves/Valve Parts Features: Chemical Resistant; Creep Resistant; Good Dimensional Stability; Good Stiffness; High Heat Resistance; High Strength; High Temperature Strength; Low Moisture Absorption Injection notes: Storage: - Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide. Information provided by Solvay Specialty Polymers. |