MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lehvoss LUVOCOM® 3/CF/30 Nylon 66, Carbon Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Carbon Fiber Filled

Material Notes: Polyamide 6 with carbon fibers, natural color (black)

Main features: Very strong and stiff parts; low coefficient of thermal expansion. Electrically conductive, suitable for continuous discharging of statically-generated electricity.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 g/cc1.70 g/ccISO 1183-3
Water Absorption <= 1.00 %
@Time 86400 sec
<= 1.00 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.00400 - 0.00500 cm/cm0.00400 - 0.00500 in/inT(mold): 100 °C, 60x60x2 mm; ISO 294
Linear Mold Shrinkage, Transverse 0.000 - 0.00100 cm/cm0.000 - 0.00100 in/inISO max: 450 bar, 60x60x2 mm; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 220 MPa31900 psi50 mm/min; ISO 527
Elongation at Break 2.20 %2.20 %50 mm/min, Fmax; ISO 527
Tensile Modulus 21.0 GPa3050 ksi1 mm/min; ISO 527
Flexural Strength 335 MPa48600 psi10 mm/min; ISO 178
Flexural Modulus 19.0 GPa2760 ksi2 mm/min; ISO 178
Flexural Strain at Break 2.80 %2.80 %10 mm/min, Fmax; ISO 178
Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²80x10x4mm; ISO 179 1eU
Charpy Impact, Notched 4.50 J/cm²21.4 ft-lb/in²80x10x4mm; ISO 179 1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance <= 1000 ohm<= 1000 ohmRonde 60x4mm; DIN EN 62631-3-2
Insulation Resistance <= 1000 ohm<= 1000 ohmstrip electrode R25; DIN EN 62631-3-3
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C11.1 µin/in-°F10x8x4 mm; ISO 11359
Maximum Service Temperature, Air  90.0 °C
@Time 7.20e+7 sec
194 °F
@Time 20000 hour
Continuous; IEC 60216
 210 °C
@Time 720000 sec
410 °F
@Time 200 hour
during lifetime
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 270 - 280 °C518 - 536 °F
Zone 1 250 - 270 °C482 - 518 °F
Zone 2 270 - 290 °C518 - 554 °F
Zone 3 280 - 300 °C536 - 572 °F
Melt Temperature 270 °C518 °F
Mold Temperature 70.0 - 110 °C158 - 230 °F
Drying Temperature  75.0 °C
@Time 36000 - 57600 sec
167 °F
@Time 10.0 - 16.0 hour
Dehumidifying
 105 °C
@Time 14400 - 21600 sec
221 °F
@Time 4.00 - 6.00 hour
Vacuum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUU8706 / 325090

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.