MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Avient Elastamax™ XL 1092-35 TPU-Based Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP

Material Notes: This is a general purpose thermoplastic elastomer based on modified TPU technology. Physical Form: Pellet. Standard Color: Natural.

Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³ASTM D792
Melt Flow  68 g/10 min
@Load 3.80 kg,
Temperature 190 °C
68 g/10 min
@Load 8.38 lb,
Temperature 374 °F
ASTM D1238
 271.4 g/10 min
@Load 8.70 kg,
Temperature 190 °C
271.4 g/10 min
@Load 19.2 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 54545 sec. delay; ASTM D2240
Tensile Strength, Ultimate 11.2 MPa1620 psi10 in/min; ASTM D412
Elongation at Break 716 %716 %10 in/min; ASTM D412
50% Modulus 1.28 MPa
@Strain 50 %
1.28 MPa
@Strain 50 %
10 in/min; ASTM D412
100% Modulus 1.68 MPa
@Strain 100 %
244 psi
@Strain 100 %
ISO 37
200% Modulus 2.17 MPa
@Strain 200 %
315 psi
@Strain 200 %
10 in/min; ASTM D412
300% Modulus 2.75 MPa
@Strain 300 %
399 psi
@Strain 300 %
10 in/min; ASTM D412
Tear Strength 42.4 kN/m242 pliDie 'C' Tear; 20 in/min; ASTM D624
Tensile Set 10.8 %10.8 %at 100%; ASTM D412

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman AVALON® 550 B Thermoplastic Polyurethane
NEU NEUSoft™ 455-50A Ester/ether TPU / SBC blend
Lubrizol ESTANE® ETE55DT3 Ester Based Thermoplastic Polyurethane
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
NEU NEUSoft™ 597-50A Industrial Ether TPU / SBC blend

PHG856 / 46997

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.