MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Master Bond Supreme 3AN One Component, Heat Curing Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond Polymer System SUPREME 3AN is a one component, heat cured epoxy adhesive and sealant, featuring high peel and shear strength along with excellent thermal conductivity and convenient handling. SUPREME 3AN cures readily at 250°F in 20-30 minutes; and at 300°F in 5-10 minutes. Minimum curing temperature is 235°F. Being a one part system, no mixing is required and the working life is unlimited as it never cures at room temperature. The shelf life is 6 months in original closed containers. Master Bond Polymer Adhesive SUPREME 3AN produces remarkably good bonds with both high shear and high peel strength for service over a wide temperature range of -100°F to +250°F. It offers very superior resistance to impact, thermal shock, vibration and stress fatigue cracking while maintaining the moisture, creep, corrosion and heat resistance typical of epoxy resin adhesives. Master Bond Adhesive SUPREME 3AN can be applied without sagging or dripping even on vertical surfaces. It is 100% reactive and does not contain any diluents or solvents. SUPREME 3AN forms high strength and exceptionally tough bonds which are remarkably resistant to severe thermal cycling and many chemicals including water, oil, fuels, and most organic solvents even upon prolonged exposures. Adhesion to metals, glass, ceramics, wood vulcanized rubbers and many plastics is excellent. The hardened adhesive has outstanding thermal conductivity and is also a superior electrical insulator. It is widely used in aerospace, electronic, electrical, computer, automotive and chemical applications especially where convenient handling and rapid curing along with outstanding physical properties all are of critical importance.

Product Advantages:

  • Single component system; no mixing needed prior to application.
  • Ease of application; non drip application feature.
  • Versatile and rapid cure schedules; as fast as 5-10 minutes at 300°F or 20-30 minutes at 250°F.
  • High shear and peel strength to similar and dissimilar substrates over the remarkable wide temperature range of -100°F to +250°F.
  • Good electrical insulating properties and chemical resistance.
  • Superior resistance to thermal shock, impacts and stress fatigue cracking.
  • Superior durability and dimensional stability.
  • Outstanding thermal conductivity.
  • Unlimited working life, minimal waste compared to two part systems.

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 75>= 75
Tensile Modulus 3.10 GPa450 ksi
Shear Strength >= 8.27 MPa>= 1200 psiTensile, Al to Al
Peel Strength >= 1.75 kN/m>= 10.0 pliT-peel, Al to Al
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 3.31 - 3.46 W/m-K23.0 - 24.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  5.00 - 10.000 min
@Temperature 149 °C
0.0833 - 0.16667 hour
@Temperature 300 °F
 20.0 - 30.0 min
@Temperature 121 °C
0.333 - 0.500 hour
@Temperature 250 °F
Shelf Life 6.00 Month
@Temperature 23.9 °C
6.00 Month
@Temperature 75.0 °F
in original closed containers
 
Descriptive Properties
AppearanceGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTB355 / 149602

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.