MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eagle Brass 735 Nickel Silver 18%, 1/4 Hard
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.

Information provided by Eagle Brass Company

Key Words: UNS C73500, ASTM B122
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.83 g/cc0.319 lb/in³Annealed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell 30T 60 - 7060 - 70Thickness > 0.020 Inch
Tensile Strength, Ultimate 386 - 476 MPa56000 - 69000 psi
Tensile Strength, Yield 193 - 400 MPa28000 - 58000 psi0.2% offset
Elongation at Break 10 - 25 %10 - 25 %in 2 in.
Tensile Modulus 124 GPa18000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000223 ohm-cm0.0000223 ohm-cmAnnealed
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 37.2 W/m-K258 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 72 %72 %
Nickel, Ni 18 %18 %
Zinc, Zn 10 %10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eagle Brass 735 Nickel Silver 18%, 1/2 Hard
Beryllium Copper, UNS C17200, TH04 Temper Strip
Haynes Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated
Eagle Brass 735 Nickel Silver 18%, Annealed
Eagle Brass 735 Nickel Silver 18%, Spring

NEAGLE194 / 147443

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.