MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Tabriz HD 4005EA High Density Polyethylene Copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: HD4005EA is high density polyethylene copolymer containing butene-1(C4) as comonomer. It is suitable for use as pipe coating applications. Applications: pipe coating applications HD4005EA has good impact strength and chemical resistance, high ESCR

Information provided by Tabriz Petrochemical Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D1505
ESCR 10% Igepal® >= 1000 hour>= 1000 hourF20; ASTM D1693A
Oxidative Induction Time (OIT) 45 min45 minASTM D3895
Melt Flow 0.50 g/10 min
@Load 2.16 kg
0.50 g/10 min
@Load 4.76 lb
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 26.0 MPa3770 psiASTM D638
Tensile Strength, Yield 17.0 MPa2470 psiASTM D638
Elongation at Break 600 %600 %ASTM D638
Charpy Impact, Notched NBNBASTM D6110
 
Thermal PropertiesMetricEnglishComments
Melting Point 125 °C257 °FASTM D-1525
Vicat Softening Point 115 °C239 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) EX 3 - 80 High Density Polyethylene
Iran Petrochemical (PCC) EX 3 – 100S HM CRP 100 N High Density Polyethylene
Ineos K38-20-138 Pipe Extrusion Grade Polyethylene
Tabriz HD 4440EA High Density Polyethylene Copolymer
Kazanorgsintez PE2NT 11-285D High Density Polyethylene Composite

PTABRZ912 / 198223

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.