MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil LD 313.NF Blown Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: LD 313.NF is a 3 wt% vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopolymers.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.925 g/ccExxonMobil Method
Vinyl Acetate Content 3.0 %ExxonMobil Method
Thickness 1.50 mil
Melt Flow 2.5 g/10 minExxonMobil Method
Antiblock Level 2500 ppm
Slip Level 800 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 230 %ASTM D882
Film Elongation at Break, TD 580 %ASTM D882
Elmendorf Tear Strength MD 240 gASTM D1922
Elmendorf Tear Strength TD 140 gASTM D1922
Elmendorf Tear Strength, MD 160 g/milASTM D1922
Elmendorf Tear Strength, TD 93.33 g/milASTM D1922
Dart Drop 93.3 g/milASTM D1709
Dart Drop Test 140 gASTM D1709
Film Tensile Strength at Break, MD 3330 psiASTM D882
Film Tensile Strength at Break, TD 3010 psiASTM D882
1% Secant Modulus, MD 23800 psiASTM D882
1% Secant Modulus, TD 27200 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 °FPeak Melting Temperature; ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Haze 5.7 %ASTM D1003
Gloss 75 %45°; ASTM D2457
 
Descriptive Properties
FeaturesThermal Stabilizer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials Pearlthane® MB-51UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlthane® MB-9010 Thermoplastic Polyurethane Elastomer
Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Total EVA 1010 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film
Versalis Greenflex® FF 35 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion

PEXB013 / 37318

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.