MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips 66 Syncon® 220 Synthetic R&O Oil
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear drives and other industrial equipment operating under severe-service conditions or at extreme temperatures. It is particularly recommended for use in applications where operating conditions may be unfavorable or too severe for conventional mineral oil-based circulating oils. Syncon R&O Oil is formulated with synthetic polyalphaolefin(PAO) base oils and select additives to provide excellent protection against rust, corrosion and deposit formation. It has outstanding oxidation resistance and thermal stability at high temperatures to minimize sludge and varnish formation, and provide long service life. It protects system components against rust, corrosion and wear. It has excellent low-temperature properties for use over a wide temperature range, and is resistant to excessive foam buildup that can interfere with proper lubrication. Syncon R&O Oil is compatible with mineral oil-based lubricants, but mixing should be avoided for optimum performance benefits.

Applications:

  • Rotary air compressors where the manufacturer specifies a PAO-based lubricant
  • Plain and rolling-element bearings operating at very high or very low temperatures
  • Lightly to moderately loaded enclosed industrial gear drives that do not require a compounded or extreme-pressure (EP) gear lubricant
  • Circulating systems of paper machine dryer sections and calender stacks
  • Electric motor bearings
  • Industrial worm gear drives with bronze-on-steel gears
  • Lubrication of the upper cylinders of gas compressors handling natural gas or process gas (ISO VG 150 or 220, typically)
  • Vacuum pumps
  • Industrial equipment operating over a wide temperature range where an inhibited mineral oil is recommended
Features/Benefits:
  • Outstanding resistance to thermal breakdown at high temperatures
  • Outstanding oxidation resistance to minimize sludge and varnish formation
  • Protects against wear
  • Protects against rust and corrosion
  • Good water-separating properties
  • Good foam resistance
  • Excellent low-temperature fluidity
  • Low carbon-forming tendency for use in rotary air compressors
  • Extended service intervals compared with conventional mineral oil-based lubricants
  • Compatible with mineral oil-based lubricants

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.875 g/cc
Density 7.29 lb/gal
Viscosity Measurement 127Viscosity Index
Saybolt Viscosity at 100°F 1150 SUS
Saybolt Viscosity at 210°F 114 SUS
Kinematic Viscosity at 40°C (104°F) 220 cSt
Kinematic Viscosity at 100°C (212°F) 22.8 cSt
Oxidative Stability 14.17 hourRPVOT; ASTM D2272
ASTM Color 1.0L; ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.20[mg KOH/g]; ASTM D974
 
Mechanical PropertiesOriginal ValueComments
Four Ball Wear 0.400 mmScar Diameter; ASTM D4172
 
Thermal PropertiesOriginal ValueComments
Pour Point -37.0 °F
Flash Point 475 °FCOC
 
Descriptive Properties
ASTM Rust A&BPass
Copper Corrosion1BASTM D130
FZG Scuffing Test10 Failure Load StageASTM D5182

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON177 / 75214

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.