MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Akoafloor PB R 509 BROWN
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Akoafloor, a PB-1 based copolymer (PB-R), has been designed to meet the growing demand for flexible pipes in surface heating and cooling systems. These random copolymers provide higher flexibility thus facilitating easier installation. Additionally, PB-R copolymers offer marked improvement in elongation at break and impact toughness allowing for quicker installation at lower temperatures with a lower risk of damage. Akoafloor PB R 509 brown is a highly isotactic random copolymer manufactured from butene-1 monomer. The product provides good long term hydrostatic strength also at elevated temperatures combined with extremely high flexibility. Akoafloor PB R 509 complies with requirements specified in ISO 12230, DIN 16968/DIN 16969 for PB-1 pipe applications. The grade is typically used for under floor heating or surface cooling applications. Akoafloor PB R 509 is available in brown color in pellet form. Akoafloor PB R 509 may not be used in the manufacture of pipe applications intended for sale or shipment to North America, without prior written approval by manufacturer for each specific product and application. Applications: Underfloor Heating

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.925 g/cc0.0334 lb/in³ISO 1183-1
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 35.0 MPa5080 psiISO 8986-2
Tensile Strength, Yield 15.0 MPa2180 psiISO 8986-2
Elongation at Break 320 %320 %ISO 8986-2
Flexural Modulus 0.370 GPa53.7 ksiISO 178
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 190 °C347 - 374 °FExtrusion Temperature
 200 - 240 °C392 - 464 °FInjection Molding Temperature
 
Descriptive Properties
Cooling Water Temperature (°C)10 to 12
Processing MethodPipe, Sheet
Vacuum (mbar)30 to 60

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQT7052 / 218690

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.