MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Toray PMC CFRT® TW-1000 w/401EB® Thermoplastic Composite Laminate
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Polyurethane, TP

Material Notes: Toray PMC CFRT® (TW-1000 w/401EB®) is a reinforced thermoplastic composite laminate. It blends the benefits of a thermoplastic polymer matrix with woven carbon and glass fibers in a twill weave for enhanced shapes and performance. The TW-1000 w/401EB® style laminate is available in a single-layer product; carbon in one direction and glass fibers at a 90° orientation to the carbon that is ultra-thin, lightweight, and resilient for improved energy return. ENVIR-Bond® is TPMC’s newest material innovation to improve the ease of processing at the factory level and help reduce the amount of harmful solvents used in the footwear manufacturing process. EB® “tie-layers” are added for injection overmolding.

Features:

  • Twill weave of carbon and glass fibers
  • Bi-directional reinforcement
  • Highest mechanical properties of our woven fabrics
  • Lightest weight, thin, single layers
  • Available in stock and custom colors
Product Type And Composition: Carbon fiber content: 20%; Glass fiber content: 20%; TPU/PMMA proprietary thermoplastic resin: 48%; Polyurethane Based Coating: 12% (Nominal volume percentages)

Typical Applications:

  • Footwear
  • Recreational equipment
  • Skates

Information provided by Toray Performance Materials Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 - 1.60 g/cc0.0506 - 0.0578 lb/in³
Thickness 900 - 1200 microns35.4 - 47.2 mil
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength >= 140 MPa
@Thickness 1.09 mm
>= 20300 psi
@Thickness 0.0429 in
ASTM D790-10
Flexural Modulus 7.00 GPa
@Thickness 1.09 mm
1020 ksi
@Thickness 0.0429 in
ASTM D790-10
 
Processing PropertiesMetricEnglishComments
Processing Temperature 55.0 - 60.0 °C131 - 140 °FBonding
 195 - 200 °C383 - 392 °FForming
 
Descriptive Properties
ColorsSilver, Charcoal, and Black
Flexural Rigidity< 80 N-cm1.09 mm, ASTM D790-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTORAY8076 / 265474

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.