Fair to excellent corrosion resistance. Excellent cold workability; good hot formability. Applications: radiator cores and tanks, flashlight shells, lamp fixtures, fasteners, locks, hinges, ammunition components, plumbing accessories, pins, rivets. Test specimens: flat products - 1mm thick and tubing - 2mm OD x 1.6mm thickness |
70/30 brass, CDA 260, CZ106, ISO CuZn30, CEN CW505L |