MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Adamas Adalon® 118 PTFE, 23/2% Carbon/Graphite Filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Carbon Fiber Filled

Material Notes:

Information provided by Adamas, HPM

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.06 - 2.10 g/ccASTM D792
Deformation 2.0 - 3.9 %Permanent deformation after 24 hrs @ 23°C; ASTM D621
 5.0 - 6.9 %ASTM D621
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 58 - 62ASTM D2240
Tensile Strength at Break >= 14.0 MPaASTM D4745-11
Elongation at Break >= 90 %ASTM D4745-11
Compressive Strength >= 10.0 MPa
@Temperature 23.0 °C,
Time 86400 sec
@ 1% deformation, 140 Kg/cm2; ASTM D621
Coefficient of Friction, Dynamic 0.10 - 0.12ASTM D1894
Coefficient of Friction, Static 0.14 - 0.16ASTM D1894
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 10000 ohm-cmASTM D257
Surface Resistance 1000 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.280 W/m-KASTM C 177
Melting Point 327 °CDSC
Maximum Service Temperature, Air 260 °CDSC
Minimum Service Temperature, Air -80.0 °CDSC
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Dyneon™ CC503 Custom Fluoropolymer Compound
3M Dyneon™ CC605 Custom Fluoropolymer Compound
Adamas Adalon® 113 PTFE, 23/2% Carbon/Graphite Filled
Celanese Nilit FRIANYL B63 CV20 Nylon 6.6 for injection molding, 20% carbon fiber reinforced
Ensinger Tecatron® XP-85 Compression Molded PPS Compound, with 30% Carbon Fiber

PHADAM006 / 147199

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.