MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SunChemical Gwent D2030506D3 Low Temperature Polymer Dielectric  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: D2030506D3 low temperature cure dielectric is suitable for use as an insulating layer when printed onto untreated aluminum, glass or alumina substrates. It is compatible with a range of silver and carbon curing systems in order to construct simple circuits. This material gives a clear film when printed.

These products are based on a unique curing process that results in the low temperature formation of a thermosetting insulation ink that combines good adhesion and insulation resistance with chemical, environmental and abrasion resistance. They offer the advantage of a One-Pack cure system combined with the convenience of ambient temperature stability and cure temperatures in the range of 130-180°C.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size <= 1.0 µm<= 1.0 µm3rd Streak; Fineness of Grind
 <= 1.0 µm<= 1.0 µmMain Break; Fineness of Grind
Viscosity 5000 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
5000 cP
@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT550 cone and plate viscometer (PK1.1°)
Storage Temperature 20.0 °C68.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 250 °C482 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min
@Temperature 150 °C
1.00 hour
@Temperature 302 °F
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Coverage cm2/g500230 mesh stainless steel screen
Printing Mesh counts/inch120 to 230stainless steel or polyester screens

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WGEM032 / 75885

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.