MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Wolf Kunststoff INKUFORM CTF H4T
Categories: Polymer; Thermoplastic

Material Notes:

Information provided by Wolf Kunststoff

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.53 g/ccISO 1183
Water Absorption 0.64 %RMC 93%; DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80DIN 53505
Ball Indentation Hardness 118 MPaH358/30; DIN 2039
Tensile Strength, Yield 47.0 MPaDIN EN ISO 527
Elongation at Break 16 %DIN EN ISO 527
Elongation at Yield 7.0 %DIN EN ISO 527
Tensile Modulus 2550 MPaDIN EN ISO 527
Flexural Modulus 2352 MPaDIN EN ISO 178
K Factor (ISO) 0.58 µm/km
@Temperature 20.0 °C
Charpy Impact, Notched 4.00 kJ/m²EN ISO 179/1eA
Coefficient of Friction, Dynamic 0.089
@Temperature 20.0 °C
Coefficient of Friction, Static 0.108
@Temperature 20.0 °C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 3.6
@Frequency 110 Hz
IEC 250
Dielectric Strength 33.0 kV/mmIEC 243
Dissipation Factor 0.0021
@Frequency 110 Hz
IEC 112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 108 µm/m-°C
@Temperature 100 °C
ISO E 830
Melting Point 169 °C
Maximum Service Temperature, Air 100 °Clong term; UL 746B
 140 °C3 h
Deflection Temperature at 1.8 MPa (264 psi) 100 °CDIN EN ISO 75
Flammability, UL94 HB
@Thickness 3.20 mm
 
Descriptive Properties
ColorWhite
Injection molded partsApplicable
Plastic granulesApplicable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZEDEX3011 / 250068

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.