MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Envalior Durethan® TP 036-052 000000 Nylon 6, 60% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 60% Glass Fiber Filled

Material Notes: PA 6, injection molding grade, 60% glass fibers, good flowability (Easy Flow), good heat-resistance

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 159 MPa23100 psiConditioned; ISO 527-1/-2
 240 MPa34800 psiISO 527-1/-2
Elongation at Break 2.6 %2.6 %ISO 527-1/-2
 3.8 %3.8 %Conditioned; ISO 527-1/-2
Tensile Modulus 12.5 GPa1810 ksiConditioned; ISO 527-1/-2
 19.3 GPa2800 ksiISO 527-1/-2
Impact 4.34.3Puncture maximum force (N); ISO 6603-2
 3.8
@Temperature -30.0 °C
3.8
@Temperature -22.0 °F
Puncture maximum force (N); ISO 6603-2
Puncture Energy 1476 J1089 ft-lbISO 6603-2
 1346 J
@Temperature -30.0 °C
992.8 ft-lb
@Temperature -22.0 °F
ISO 6603-2
 1346 J
@Temperature -30.0 °C
992.8 ft-lb
@Temperature -22.0 °F
Conditioned; ISO 6603-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C5.56 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C50.0 µin/in-°FISO 11359-1/-2
Melting Point 221 °C430 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 213 °C415 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 186 °C367 °FISO 75-1/-2
 
Descriptive Properties
FeaturesHeat stabilized or stable to heat
FormPellets
ProcessingInjection molding
RegionAsia Pacific
 Europe
 Near East/Africa
 North America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® TP 142-011 900116 Nylon 6

PLANX0835 / 99050

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.