MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Lucas-Milhaupt Silvaloy® 401
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Braze 401 is an intermediate temperature filler metal that may be used as a cadmium free substitute for Easy-Flo 30 or used in applications where an intermediate silver-copper-zinc alloy is needed. It liquates moderately, but this property is useful in bridging gaps where poor joint fitup cannot be avoided. It flows well on steels, copper and copper alloys. The use of Handy Flux or Handy Flux Type B-1 is recommended.

Applications:Braze 401 is a good general purpose, intermediate temperature brazing alloy for use on copper, brass, nickel-silver, bronze and other nonferrous alloys as well as mild steel, stainless steel, nickel and Monel metal.

Specifications:This filler metal conforms to the following specifications-SAE AMS-4762.

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.99 g/cc0.325 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 232 MPa33700 psiCopper but joint
 556 MPa80700 psi1020 Carbon Steel butt joint
 587 MPa85100 psi304 Stainless Steel butt joint
Elongation at Break 2.4 %2.4 %% in 2", 304 Stainless Steel butt joint
 22 %22 %% in 2", 1020 Carbon Steel butt joint
 40 %40 %% in 2", Copper butt joint
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000840 ohm-cm0.00000840 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Melting Point 673.9 - 727 °C1245 - 1340 °F
Solidus 673.9 °C1245 °FMelting Point
Liquidus 727 °C1340 °FFlow Point
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 29 - 31 %29 - 31 %
Other, total <= 0.15 %<= 0.15 %
Silver, Ag 39 - 41 %39 - 41 %
Zinc, Zn 28 - 32 %28 - 32 %
 
Descriptive Properties
ColorPale Yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucas-Milhaupt Silvaloy® 450 Silver Based Cadmium Free Filler Metal
Materion Beryllium Copper Alloy 10 Rod and Bar; H (TD04) Temper; up to 76 mm (UNS C17500)
Materion Beryllium Copper Alloy 10 Forgings & Extrusions; AT (TF00) Temper (UNS C17500)
Lucas-Milhaupt Silvaloy® 560 (Braze™ 560) Silver-Copper-Zinc Alloy (AWS BAg-7)
Lucas-Milhaupt Silvaloy® 452

NLUCMI14 / 18081

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.