MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics CHO-SEAL 1285R Reinforced Conductive Elastomer Seal  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at joints, seams and openings for radar cross section reduction.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 - 2.10 g/cc1.60 - 2.10 g/ccASTM D792
 1.65 - 2.15 g/cc1.65 - 2.15 g/ccBase Material; ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565Base Material; ASTM D2240
Tensile Strength at Break >= 1.38 MPa>= 200 psiBase Material; ASTM D412
 2.41 MPa350 psiReinforced Material - Fill; ASTM D412
 4.48 MPa650 psiReinforced Material, warp; ASTM D412
Elongation at Break >= 50 %>= 50 %Reinforced Material - Fill/Warp; ASTM D412
 >= 100 %>= 100 %Base Material; ASTM D412
Tear Strength 5.25 kN/m30.0 pliBase Material; ASTM D624
 35.0 kN/m200 pliReinforced Material - Warp/Fill; ASTM D624
Compression Set 32 %
@Temperature 100 °C,
Time 252000 sec
32 %
@Temperature 212 °F,
Time 70.0 hour
ASTM D395
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0080 ohm-cm0.0080 ohm-cmReinforced Material; MIL-G-83528
 0.0080 ohm-cm0.0080 ohm-cmBase Material; MIL-G-83528
 <= 0.015 ohm-cm<= 0.015 ohm-cmPost Tensile Strength; MIL-G-83528
Shielding Effectiveness >= 60 dB>= 60 dB200 kHz (H Field) - Base/Reinforced Material; MIL-G-83528
 >= 100 dB>= 100 dB10 GHz (Plane Wave) - Base/Reinforced Material; MIL-G-83528
 >= 105 dB>= 105 dB2 GHz (Plane Wave) - Base/Reinforced Material; MIL-G-83528
 >= 110 dB>= 110 dB500 MHz (E Field) - Base/Reinforced Material; MIL-G-83528
 >= 115 dB>= 115 dB100 MHz (E Field) - Base/Reinforced Material; MIL-G-83528
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 160 °C320 °F
Minimum Service Temperature, Air >= -65.0 °C>= -85.0 °FLow Temp Flex - Base Material, TR10
 >= -65.0 °C>= -85.0 °FLow Temp Flex - Reinforced Material, TR10
 
Descriptive Properties
BinderSilicone, Base Material
EMP Survivability kA / in, min0.9
FillerAg/Al, Reinforced Material
GradeMilitary-Aerospace
Heat Aging - Base Material ohm-cm max0.01
Heat Aging - Reinforced Material ohm-cm max0.01
Vibration Res, After - Base Material ohm-cm max0.008
 0.008
Vibration Res, During - Base Material ohm-cm max0.012
 0.012

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NuSil EPM-2463 Silicone, Thermal Interface Material (TIM): Electrically Conductive
NuSil R-2634 Silicone, Electrically Conductive
P & P Technology EC-S Pure Silver Loaded Silicone
Parker Chomerics CHO-SEAL 1221 Conductive Elastomer
Parker Chomerics Tecknit Consil®-R 855 Pure Silver-Filled Silicone Elastomer

PCHOME123 / 28345

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.