MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik Laurolactam
Categories: Other Engineering Material

Material Notes: CAS No: 947-04-6

Laurolactam (LL) is a colorless solid at room temperature. It is readily soluble in organic solvents but has only limited solubility (0.03% by weight) in water at 20°C

  • LL mainly provides the basis for the production of PA 12 (VESTAMID® L).
  • It is also used as a co-monomer in polyamide 6.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Molecular Weight 197.32 g/mol197.32 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 151.5 °C304.7 °F
Boiling Point 158 °C
@Pressure 0.000100 MPa
316 °F
@Pressure 0.0145 psi
 
Descriptive Properties
Color<30 mg Pt/lAPHA, Solution color
 <300 mg Pt/lAPHA, Melt color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIL715 / 196919

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.