MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

HB Fuller Swift®lock 9053 Hot melt Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Suggested Application: 9053 is a single-component, fully reactive hot melt adhesive that cross-links through a chemical reaction with moisture found in the surrounding air and substrates, to produce a thermoset adhesive. 9053 was specifically formulated for use in the assembly of recreational vehicle subcomponents, including skins, composite walls, floors, ceilings and front caps. Substrates typically bonded include FRP, aluminum, lauan and other plywoods. Cutting edge technology allows 9053 to quickly build green strength while simultaneously delivering extended open time often necessary for assembling large and complex components. 9053 unique formulation also provides fiber tearing bonds very quickly, as well as providing deep foam tear at -20ºF, room temperature and 180 ºF. It is blue in color and very visible, so the use of black lights or UV indicators is not required.

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 22000 - 28000 cP
@Temperature 121 °C
22000 - 28000 cP
@Temperature 250 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 13.1 - 14.5 MPa1900 - 2100 psi
Elongation at Break 450 - 550 %450 - 550 %
2% Secant Modulus 0.0283 - 0.0296 GPa4.10 - 4.30 ksi
 
Processing PropertiesMetricEnglishComments
Cure Time 7.00 min0.117 hourOpen Time
 240 min4.00 hour0.75
 
Descriptive Properties
ColorBright Blue Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL163 / 316954

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.